A chemosensitive-based ammonia gas sensor with PANI/PEO–ZnO nanofiber composites sensing layer

Gözde Konuk Ege (Department of Mechatronics, Gedik Vocational School, Istanbul Gedik University, Istanbul, Turkey)
Özge Akay (Department of Mechatronics Engineering, Faculty of Technology, Marmara University, Istanbul, Turkey)
Hüseyin Yüce (Department of Mechatronics Engineering, Faculty of Technology, Marmara University, Istanbul, Turkey)

Microelectronics International

ISSN: 1356-5362

Article publication date: 15 May 2023

125

Abstract

Purpose

This study aims to investigate the ammonia-sensing performance of polyaniline/polyethylene oxide (PANI/PEO) and polyaniline/polyethylene oxide/zinc oxide (PANI/PEO-ZnO) composite nanofibers at room temperature.

Design/methodology/approach

Gas sensor structures were fabricated using microfabrication techniques. First, onto the SiO2 wafer, gold electrodes were fabricated via thermal evaporation. PANI/PEO nanofibers were produced by the electrospinning method, and the ZnO layer was deposited by using radio frequency (RF) magnetron sputtering on the electrospun nanofibers as a sensing layer. Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM) and X-ray diffraction were performed to characterize the analysis of nanofibers. After all, gas sensing analysis of PANI/PEO and PANI/PEO/ZnO nanofibers was conducted using an experimental setup at room temperature conditions. Furthermore, the impact of humidity (17%–90% RH) on the sensor resistance was actively investigated.

Findings

FTIR analysis confirms the presence of functional groups of PANI, PEO and ZnO in nanofiber structure. SEM micrographs demonstrate beads-free, thinner and smooth nanofibers with ZnO contribution to electrospun PANI/PEO nanofibers. Moreover, according to the gas sensing results, the PANI/PEO nanofibers exhibit 115 s and 457 s response time and recovery time, respectively. However, the PANI/PEO/ZnO nanofibers exhibit 245 s and 153 s response time and recovery time, respectively. PANI/PEO/MOx composite nanofibers ensure stability to the NH3 gas owing to the high surface/volume ratio and decrease in the humidity dependence of gas sensors, making gas sensors more stable to the environment.

Originality/value

In this study, ZnO was deposited via RF magnetron sputtering techniques on PANI/PEO nanofibers as a different approach instead of in situ polymerization to investigate and enhance the sensor response and recovery time of the PANI/PEO/ZnO and PANI/PEO composite nanofibers to ammonia. These results indicated that ZnO can enhance the sensing properties of conductive polymer-based resistive sensors.

Keywords

Citation

Konuk Ege, G., Akay, Ö. and Yüce, H. (2023), "A chemosensitive-based ammonia gas sensor with PANI/PEO–ZnO nanofiber composites sensing layer", Microelectronics International, Vol. ahead-of-print No. ahead-of-print. https://doi.org/10.1108/MI-04-2023-0051

Publisher

:

Emerald Publishing Limited

Copyright © 2023, Emerald Publishing Limited

Related articles