Forming limit diagram and optimization of process parameters in SPIF of Inconel 625 aviation-grade superalloy
Aircraft Engineering and Aerospace Technology
ISSN: 0002-2667
Article publication date: 10 October 2023
Issue publication date: 6 February 2024
Abstract
Purpose
This paper aims to optimize the single-point incremental forming process variables for realizing higher formability in Inconel 625 components and to plot the forming limit diagram for Inconel 625 aviation-grade superalloy.
Design/methodology/approach
The formability of Inconel 625 components has been measured in terms of major strain, minor strain and minimum sheet thickness. Response surface methodology with desirability function analysis has been used to achieve maximum formability. The finite element analysis has been conducted at optimal parametric setting.
Findings
The derived forming limit diagram proves that the maximum forming limit for Inconel 625 is 57.5° at the optimal parametric setting, achieved with desirability of 0.995. The outcomes of finite element analysis conducted at optimal parametric setting show excellent agreement with confirmation experiment results.
Practical implications
Inconel 625 superalloy is frequently used in aircraft and other high-performance applications for its superior strength.
Originality/value
It has been suggested that to enhance formability, higher tool rotation speed, minimum step-size, larger tooltip diameter and higher wall angle must be used. Wall angle is the governing parameter among all the parameters.
Keywords
Acknowledgements
The authors would like to acknowledge the National Institute of Technology Kurukshetera, Haryana, India for providing the facilities required to carry out this research work.
Citation
Bishnoi, P. and Chandna, P. (2024), "Forming limit diagram and optimization of process parameters in SPIF of Inconel 625 aviation-grade superalloy", Aircraft Engineering and Aerospace Technology, Vol. 96 No. 1, pp. 84-95. https://doi.org/10.1108/AEAT-07-2023-0179
Publisher
:Emerald Publishing Limited
Copyright © 2023, Emerald Publishing Limited