LABORATORY TESTING FOR STRESS CORROSION CRACKING
Abstract
Introduction The ever increasing demands made on materials by advanced technology has led, in recent years, to a greater awareness of the importance of mechano‐chemical behaviour. These may be defined as the synergistic effect of mechanical forces and chemical reactions on the material. Although possibly interrelated, three classes of mechano‐chemical reactions have been identified as; stress‐corrosion (SCC), corrosion fatigue (CF) and hydrogen embrittlement. SCC has become one of the ‘in’ subjects of corrosion science during the last decade, while the importance of CF has emerged comparatively recently. In a review of the national corrosion and protection scene in 1970, it was revealed that 62 postgraduate research workers, representing 21% of the total effort in the corrosion and protection field, were involved in mechano‐chemical corrosion studies1. The bulk of these were working on SCC. This large research effort has not resulted in a standardisation of test methods nor, despite several attempts, in a unifying theory for SCC2. The newcomer to the field is faced with a bewildering variety of tests of varying complexity and validity. The supporters of each type of test tend to make exaggerated claims particularly when the test they are advocating is the only one which has caused a particular alloy‐environment system to exhibit SCC.
Citation
Brettle, J. and Orman, S. (1973), "LABORATORY TESTING FOR STRESS CORROSION CRACKING", Anti-Corrosion Methods and Materials, Vol. 20 No. 9, pp. 3-10. https://doi.org/10.1108/eb006928
Publisher
:MCB UP Ltd
Copyright © 1973, MCB UP Limited