Zulmiardi and Meriatna

Results – From a hardening test, we then tested with an impact tester charpy Treviolo H060. The results showed that the impact strength is escalated up to 29.09% post-hardening…

Abstract

Results – From a hardening test, we then tested with an impact tester charpy Treviolo H060. The results showed that the impact strength is escalated up to 29.09% post-hardening circle, which was observed using electrical microscope. The value of steel strength increased 2.12 J/mm2 compared with earlier hardening process, which is, 1.57 J/mm2. The results showed that the fracture in the welding process without the hardening process is a brittle fracture that is shown by the flat crystal structure; on the other hand, the hardening process before welding shows a form of coarse-looking structure indicating that the specimen has an impact towards which the toughness is higher.

Research Limitations/Implications – The effect influence of the hardening process to the impact strength of welded joints before and after the hardening process SMAW AISI 1050 steel hardening process. The mechanical properties test is done with the equipment impact charpy.

Practical Implications – The field we often encounter is erosion or wear out occurring in the construction, for example, many equipments such as agricultural equipment, bridges, ship construction, motor shaft, machining such as hand tools, small rings, and agricultural tools.

Originality/Value – This is the first reported research on impact strength using the hardening test.