TY - JOUR AB - Dielectric compositions with high dielectric constant, low electrical losses, high softening point and resistance to moisture and corrosive atmospheres are obtained by polymerising or copolymerising a vinyl compound containing sulphur, in a position where it is chemically and electrically stable, e.g. vinyl diphenyl sulphide, vinyl benzothiophene, vinyl oxazole, etc., or compounds in which there is oxygen present in a heterocyclic ring in which there is a vinyl substituted carbon atom, e.g. vinyl pyrane, vinyl furane, vinyl coumarone, etc. These substances are used for the production of wrapping materials, particularly for food packaging. Suitable plasticisers are given.—U.S. Pat. 2,636,022, Sprague Electric Co., L. A. Brooks, M. Markarian and M. Nazzewski. VL - 1 IS - 9 SN - 0003-5599 DO - 10.1108/eb018991 UR - https://doi.org/10.1108/eb018991 PY - 1954 Y1 - 1954/01/01 TI - CORROSION PATENTS T2 - Anti-Corrosion Methods and Materials PB - MCB UP Ltd SP - 350 EP - 350 Y2 - 2024/04/25 ER -