ELECTRON FRACTOGRAPHY OF STRESS CORROSION FRACTURE SURFACES
Abstract
Introduction Visual inspection or observation at low magnification with an optical microscope has been of great help in analysing fracture surfaces. Optical microscopy, however, has distinct limitations, such as low resolution and small depth of field. The transmission electron microscope does not have these limitations.
Citation
Van Der Vet, W.J. (1973), "ELECTRON FRACTOGRAPHY OF STRESS CORROSION FRACTURE SURFACES", Anti-Corrosion Methods and Materials, Vol. 20 No. 8, pp. 3-13. https://doi.org/10.1108/eb006925
Publisher
:MCB UP Ltd
Copyright © 1973, MCB UP Limited