To read this content please select one of the options below:

Corrosion inhibition of N80 steel in 10% HCl + 8% HBF4 solution

Juan Du (School of Petroleum and Natural Gas Engineering, State Key Lab, Southwest Petroleum University, Chengdu, China)
Yuning He (School of Petroleum and Natural Gas Engineering, State Key Lab, Southwest Petroleum University, Chengdu, China)
Pingli Liu (School of Petroleum and Natural Gas Engineering, State Key Lab, Southwest Petroleum University, Chengdu, China)
Yigang Liu (CNOOC China Co. Ltd, Tianjin, China)
Xianghai Meng (CNOOC China Co. Ltd, Tianjin, China)
Liqiang Zhao (School of Petroleum and Natural Gas Engineering, State Key Lab, Southwest Petroleum University, Chengdu, China)

Anti-Corrosion Methods and Materials

ISSN: 0003-5599

Article publication date: 2 November 2018

Issue publication date: 24 January 2019

202

Abstract

Purpose

This paper aims to analyze the corrosion and corrosion inhibition of N80 in 10 per cent HCl + 8 per cent fluoroboric acid (HBF4) solution for acidizing operation.

Design/methodology/approach

The corrosion rate, kinetic parameters (Ea, A) and thermodynamic parameters (ΔH, ΔS) of N80 steel in fresh acid and spent acid, 10 per cent HCl + 8 per cent HBF4, 10 per cent HCl and 8 per cent HBF4 solutions were calculated through immersion tests. The corrosion and inhibition properties were studied through X-ray diffraction and electrochemical measurements. The corrosion morphology of the corrosion product was examined by scanning electron microscopy (SEM).

Findings

The results demonstrated that the spent acid was the main cause of acidification corrosion, and the HBF4 would cause serious corrosion to N80 steel. The results showed that the N80 steel was more seriously corroded in the spent acid than in fresh acid, and the hydrolysis of HBF4 accelerates the dissolution process of N80 steel anode to control the corrosion reaction. The results showed that the acidification will definitely cause serious corrosion to the oil tube; therefore, necessary anti-corrosion measures must be taken in the acidification process.

Originality/value

The results showed that acidizing the formation with 10 per cent HCl + 8 per cent HBF4 will definitely cause serious corrosion to the oil tube, especially when the spent acid flows back. Therefore, necessary anti-corrosion measures must be taken in the acidification process, especially in the spent acid flowback stage.

Keywords

Acknowledgements

The work in this paper was supported by National Science and Technology Major Project of the Ministry of Science and Technology of China (High Efficiency Oil Production and Supporting Technology Demonstration in Bohai Oilfield, and the No. 2016ZX05058-003).

Citation

Du, J., He, Y., Liu, P., Liu, Y., Meng, X. and Zhao, L. (2019), "Corrosion inhibition of N80 steel in 10% HCl + 8% HBF4 solution", Anti-Corrosion Methods and Materials, Vol. 66 No. 1, pp. 1-10. https://doi.org/10.1108/ACMM-01-2018-1883

Publisher

:

Emerald Publishing Limited

Copyright © 2018, Emerald Publishing Limited

Related articles