Studies on the pitting corrosion of lead in carbonate media

E.E. Abd El Aal (Chemistry Department, Faculty of Science, Zagazig University, Zagazig, Egypt)

Anti-Corrosion Methods and Materials

ISSN: 0003-5599

Article publication date: 1 April 2001

402

Abstract

Cyclic voltametry and potentiodynamic single sweep techniques are used to study the electrochemical behaviour of lead in Na2CO3 solutions containing various concentrations of ClO4 as aggressive anion. The effects of different concentrations, in terms of destruction of passivity and initiation of pitting corrosion, were monitored with reference to the change in integrated anodic charge. It was found that Δqa (taken as a measure of the extent of pitting) varies linearly with log CClO4. The pitting corrosion potential, Epitting, varies with log CClO4 according to sigmoidal curves. These curves are explained on the basis of formation of passive, active and continuously propagating pits. Additions of aliphatic amines shift the pitting corrosion potential, Epitting, into the noble (positive) direction, indicating the inhibition action of the added amines on the pitting attack. Epitting varies with the logarithm of the inhibitor concentration according to: Epitting = a + b log Cinh. The inhibition of pitting corrosion by the aliphatic amines is assumed to be due to either competitive adsorption between the CO32– with ClO4 anions, and/or the chemisorption of the amine on the metal with the formation of a metal‐nitrogen coordination bond. The efficiency of these compounds as pitting corrosion inhibitors increases with the increase in the chain length of the alkyl group.

Keywords

Citation

Abd El Aal, E.E. (2001), "Studies on the pitting corrosion of lead in carbonate media", Anti-Corrosion Methods and Materials, Vol. 48 No. 2, pp. 116-126. https://doi.org/10.1108/00035590110384119

Publisher

:

MCB UP Ltd

Copyright © 2001, MCB UP Limited

Related articles